Silicon Monocrystalline
1. Crystal growth method The Chohralsky
2. Diameter mm 152,5±1,0
3. Length of an ingot mm 150-550
4. Polarity of conductivity,
alloying impurity P,
Boron
5. Orientation crystallographic ingot...
Scrap Of Silicon Monocrystalline
1. The minimum weight of a piece, not less Gramme 30
2. Polarity of conductivity P-type (Boron)
3. Specific resistance (R) Ohm * sm -3 0,5-3
4. Concentration of carbon, no more At/sm-3 1*1017
5....